During Using
hand-lay FRP product, the surface severe frost or yellowing. Causes and
prevention measures are as follows:
The main reason
and solution for bleaching:
1, the gel coat
resin is not completely cured, appropriate changes in the ratio of hardener
systems and usage.
2, pigment or
filler improper selection or excessive amount, must strictly control the
dosage.
3, resin
formulations wrong, does not apply to the conditions of use, it must be
properly selected resin formulations.
4, resin or
fibers mixed with water, too much humidity operating environment, must overcome
aerodynamic influence of moisture or wet.
Yellowing causes
and solutions
1, the speed of the
working chamber is too large, or reinforcing material too dry, the working
environment should ensure that the raw materials with dry and low humidity;
2, resin wrong
or incomplete curing, stability of the resin should be used to make products
entirely cured before use;
3, Using benzoyl
peroxide and amine accelerators easy to turn yellow, and if use too much
peroxide methyl ethyl ketone and colorless accelerators it will be better.